Thread | Coating Height | Diameter(MM) | Cooling lubricant | Drilling Materail | Drilling Method | Machine |
M14 | 10MM | 6 | Yes | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 8 | Yes | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 10 | Yes | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 12 | Yes | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 14 | Yes | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 18 | Yes | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 20 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 25 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 27-95 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 100 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 105 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 110 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 115 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
M14 | 10MM | 120 | No | Ceramic/Stone | Drilling without Water | Angle grinder |
With the development of National Urbanization Constriction, many problems have to be solved in the engineering construction and emergency rescue area. High efficiency; safety and convenient cutting the high strength steel or steel-composites structure have become the major problem The application practice shows that the traditional electroplated or multi-layer sintering diamond saw blade carbide saw blades and resin grinding wheel exist abrasive fall off or tools fracture in the process of heavy load and high speed machine, which is due to the low bond strength among the abrasive ,the cutting head and the binding agent Therefore , the disadvantage of the above saw trades have seriously affected the processing efficiency safety aid service life.